| dc.creator |
CALIK, ADNAN |
|
| dc.creator |
OZBAKIR, Osman |
|
| dc.creator |
Karakas, S. |
|
| dc.creator |
UÇAR, Nazım |
|
| dc.date |
2017-01-31T21:00:00Z |
|
| dc.date.accessioned |
2020-10-06T09:49:30Z |
|
| dc.date.available |
2020-10-06T09:49:30Z |
|
| dc.identifier |
48187501-b726-4415-8e30-147f9847d71a |
|
| dc.identifier |
10.12693/aphyspola.131.252 |
|
| dc.identifier |
https://avesis.sdu.edu.tr/publication/details/48187501-b726-4415-8e30-147f9847d71a/oai |
|
| dc.identifier.uri |
http://acikerisim.sdu.edu.tr/xmlui/handle/123456789/59097 |
|
| dc.description |
In this study, pack boronizing was applied to ash-blowing nozzles manufactured from AISI 1040 steels using Ekabor II powders as the boronizing source at a temperature of 1273 K for a duration of 8 h. Erosive wear tests of boride ash-blowing nozzles were carried out in ash delivery line of thermal reactor under actual working conditions. It was observed that erosive wear resistance of borided ash-blowing nozzles were increased 3 times as a result of the boronizing process. The improved wear resistance of the borided samples can be explained by increased surface hardness and higher work hardening. |
|
| dc.language |
eng |
|
| dc.rights |
info:eu-repo/semantics/closedAccess |
|
| dc.title |
Investigation of the Erosive Wear Resistance of Boronized Ash-Blowing Nozzles |
|