| dc.description |
The orientation and temperature dependence of the work hardening rate (WHR) has been investigated in tension in the temperature range from room temperature to 500 K in Cd single crystals. The WHR was found to decrease rapidly with increasing temperature. For [2<$(11)over bar $>3] orientated crystals, the WHR increases firstly with increasing temperature until it passes a maximum at about 350 K. |
|
| dc.language |
eng |
|
| dc.rights |
info:eu-repo/semantics/closedAccess |
|
| dc.title |
Orientation and temperature dependence of work-hardening rate in Cd single crystals |
|
| dc.type |
info:eu-repo/semantics/article |
|