Isci, Devrim; ALKIŞ, Huseyin; Saglam, Aynur Medine; Elekdag-Turk, Selma; Turk, Tamer
Description:
The mean SBS was 9.01 MPa for the fluorosed teeth bonded with SEP. This value was significantly different from those of fluorosed teeth etched with PA (15.22 MPa) and non-fluorosed teeth conditioned with SEP (12.95 MPa) and PA (15.37 MPa). The ARI scores of the fluorosed teeth conditioned with SEP were significantly lower than those of non-fluorosed teeth conditioned with SEP or PA.